Fibreheart PPA-CF
Siraya Tech Fibreheart™ PPA-CF Filament
SKU ST3017
Price includes VATEarn 103 points (≈ ฿51.50)
Product features
- Evenly dispersed 15% carbon fiber
- High heat resistance (HDT up to 192°C annealed)
- Lower moisture absorption than PA6 nylon
- Strong and precise for industrial parts
- 1 kg and 2.5 kg spools
Size · 1kg
Delivery throughout Thailand.
Orders placed before 2 PM on a business day will be shipped the same day. Delivery generally takes 1-3 business days.
Shipping detailsGenuine products from manufacturers
Full tax invoices
Payment methods
- PromptPay / Thai QR Payment
- Bank Transfer
Description
Smart Fiber Reinforcement: Evenly disperses 15% carbon fibers for enhanced strength, heat resistance, and reduced warping.
Extreme Environment Durability: Exceptional thermal resistance keeps nylon-like toughness and abrasion resistance even at high temperatures.
Superior Printability: Low hygroscopicity gives better printability and dimensional stability than PA6 nylon.
Precision for Demanding Applications: The carbon fiber skeleton structure ensures accuracy in every part, ideal for automotive and industrial parts.
Before printing
- For 0.4 mm or larger nozzles only (smaller nozzles will clog)
- Hardened steel nozzle required
- Printer must have an enclosure; Bambu Lab A1 / A1 mini not recommended
- 2.5 kg spool does not fit the SUNLU E2 (fits PolyDryer Box XL)
Printing Parameters
Nozzle Temperature: 300–320°C
Bed Temperature: 70–90°C
Build Surface: PEI or PVP glue coating
Nozzle: Hardened steel, 0.4–1.0 mm
Heating Block: At least 12 mm thick
Cooling Fan: OFF
Print Speed: 30–120 mm/s
Max Volumetric Speed: 8–12 mm³/s
Retraction: 1–3 mm at 1800–3600 mm/min
Drying: 100°C for 4–6 hours (only if damp)
Technical Datasheet
Tensile Stress at Break: 95 MPa (98 annealed) · ASTM D638
Young's Modulus: 7800 MPa (8700 annealed) · ASTM D638
Elongation at Break: 2% (1.6% annealed)
Charpy Impact Strength: 11 kJ/m² (6.3 annealed) · ISO 179
Bending Strength: 145 MPa · ISO 178
Bending Modulus: 6800 MPa (7350 annealed) · ISO 178
Vicat Softening Temperature: 230°C · ISO 306
Glass Transition Temperature: 80°C
Melting Point: 232°C
HDT: 82.5°C / 119°C annealed (1.80 MPa) · 84.5°C / 192°C annealed (0.45 MPa)
Water Absorption: 1.37% · ISO 62
Density: 1.2 g/cm³
| Material | PPA (polyphthalamide) + 15% carbon fiber |
| Diameter | 1.75 mm |
| Net weight | 1 kg / 2.5 kg per spool |
| Color | Black |
| Nozzle temperature | 300–320°C |
| Bed temperature | 70–90°C |
| Nozzle | Hardened steel, 0.4 mm or larger |
| Printer | Enclosure required |
| Drying | 100°C for 4–6 h |
0 of 1 options ready to ship
| Color / option | Status | Order |
|---|---|---|
| 1kg | Out of stock | Out of stock |
Customer reviews
No reviews yet